The Influence of Multiple Welding Repairs of Pipelines in Residual Stress Assessment Related to Stress Corrosion Cracking

A. Contreras, S. L. Hernández, R. Galvan, O. Vega

Current Journal of Applied Science and Technology · pp. 621–634 · Published 9 Jan 2015

10.9734/BJAST/2015/14931

Abstract

The effect of residual stress of multiple welding repairs in seamless API 5L X52 on the stress corrosion cracking (SCC) susceptibility was evaluated. Four repairs of the girth weld were evaluated through X-ray diffraction (XRD) on the internal face of the pipe to measure residual stresses in longitudinal and circumferential direction. Residual stresses in the circumferential and longitudinal direction reach values of about 77% and 58% of the UTS (460 MPa) respectively, approaching to the YS of the steel (360 MPa). It was observed that its magnitude increases as move away from weld center line. SCC susceptibility of X52 steel welded joints with the residual stresses generated was evaluated through slow strain rate tests (SSRT) in a soil solution at low and high pH. Relation between mechanical properties and residual stresses on the SCC susceptibility was analyzed. SCC index obtained from the mechanical properties of SSRT indicate good SCC resistance of X52 steel exposed to soil solution at low and high pH. From these results, it is suggested that the region with high residual stresses before to generate cracks in the steel surface due to the combination of soil solution and the strain applied, should favor pitting formation and not cracking. Initiation of micro-cracks from these pits will depend on the geometrical form of the pit and the stresses state can be established at given pitting. It is suggested that initiation of micro-cracks from these pits may depend on the dissolution rate and morphology of the pitting and stresses on the bottom of the pitting. This favorable condition could appear increasing the soil exposition time of the steel and reducing the strain rate applied on the SSRT.  

Steel welding x-ray diffraction residual stresses stress corrosion cracking (SCC)

Cited by 17

The heat affected zone of X20Cr13 martensitic stainless steel after multiple repair welding: Microstructure and mechanical properties assessment

Mohammad Shojaati, Seyed Farshid Kashani Bozorg, Masoud Vatanara · International Journal of Pressure Vessels and Piping · 2020

On the formation of stress corrosion crack colonies with different crack population

Shidong Wang, Lyndon Lamborn, Karina Chevil · Corrosion Science · 2020

Pioneering research on the role of strain burst in the early-stage stress corrosion crack propagation

Shidong Wang, Hamed Shirazi, Hanan Farhat · Corrosion Science · 2024

Strain-Aging-Assisted Localized Corrosion of a Mill-Scaled X-65 Pipeline Steel

Shidong Wang, Lyndon Lamborn, Karina Chevil · Corrosion · 2021

Pre-cyclic-loading-enhanced Stage-1b stress corrosion crack growth of pipeline steels

Shidong Wang, Lyndon Lamborn, Weixing Chen · Corrosion Science · 2022

Experimental analysis of stresses in weld metal subjected to tensile load

Sampath S.S., Nethri Rammohan, Reema Shetty · World Journal of Engineering · 2016

Showing 8 of 17 known citations — external sources report more than can currently be individually listed.

Article metrics

Real usage data collected on this platform.

40

Page views

0

PDF downloads

4

Outbound clicks

17

Citations

Views over time

Views by country

Approximate, from request IP at view time — not citizenship or institution. Countries with fewer than 5 views are grouped as "Other".

Traffic sources

Referring site, by host.

Views and downloads exclude known bots/crawlers. Citations combines this platform's own DOI-resolved index with each external source's own reported total — see Cited by above for individually listed citing works. Last refreshed 0 seconds ago.